Waya Welding MIG Fun Irin Alagbara Irin ER308L Alurinmorin fun ọkọ ayọkẹlẹ ojò
WELDING TECHNOLOGY
Ma ṣe jẹ ki awọn ibeere
Tesiwaju lati lepa rẹ
Arc aisedeede
Iṣatunṣe aibikita
Pupọ spatter
Irin ti o dapọ ni o dara
darí-ini ati ipata resistance
O dara fun alurinmorin ti 18Cr-8Ni iru kekere-erogba alagbara, irin,
petrochemical, awọn ohun elo titẹ, ẹrọ ounjẹ, awọn ohun elo iwosan ati awọn ohun elo miiran.
Ripple itanran
Ounjẹ onirin didan, aaki iduroṣinṣin, ṣiṣẹda lẹwa
Oloomi to dara ti irin didà, asesejade kere, pẹlu iṣẹ ṣiṣe alurinmorin to dara julọ.
Rọrun slagging
Ọja Paramita
KỌMPUTA kemikali
ALOY(wt%) | C | Mn | Si | P | S | Ni | Cr | Mo | Omiiran |
GB/T OFIN | 0.017 | 0.54 | 2.06 | 0.021 | 0.012 | 9.85 | 20.03 | 0.0 | - |
Ohun-ini ẹrọ:
ONÍNÌYÀN | AGBARA YIELD(MPa) | AGBARA Ifaagun (MPa) | Ilọsiwaju/% | IMAPACT IYE J/℃ | Itọju ooru °C * h | |||||
GB/T OFIN | - | 585 | 38 | 102/-60 | - |
Niyanju welding PARAMETER:
DIAMETERS PIPICATIONS(mm) | 0.8 | 1.0 | 1.2 | ||||
ELECTRICITY (Amp) | H/W | 70-150 | 100-200 | 140-220 | |||
O/W | 50-120 | 80-150 | 120-180 |
Factory support
Ọja naa dara fun a
jakejado ibiti o ti ohun elo
WELDING TECHNOLOGY
-
GDS-2209 / GXS-E330
tube surfacing ojula
-
2.3 milionu awọn agba ti
SBM Fast4ward FPSO
-
Hainan Huasheng
ẹṣọ imularada phenol
KỌMPUTA kemikali
ALOY(wt%) | C | Mn | Si | P | S | Ni | Cr | Mo | Omiiran |
GB/T OFIN | 0.017 | 0.54 | 2.06 | 0.021 | 0.012 | 9.85 | 20.03 | 0.0 | - |
Ohun-ini ẹrọ:
ONÍNÌYÀN | AGBARA YIELD(MPa) | AGBARA Ifaagun (MPa) | Ilọsiwaju/% | IMAPACT IYE J/℃ | Itọju ooru °C * h | |||||
GB/T OFIN | - | 585 | 38 | 102/-60 | - |
Niyanju welding PARAMETER:
DIAMETERS PIPICATIONS(mm) | 0.8 | 1.0 | 1.2 | ||||
ELECTRICITY (Amp) | H/W | 70-150 | 100-200 | 140-220 | |||
O/W | 50-120 | 80-150 | 120-180 |