Awọn irin alagbara Flux Cored Waya E2209T1-1 ohun elo alurinmorin aluminiomu
WELDING TECHNOLOGY
Ma ṣe jẹ ki awọn ibeere
Tesiwaju lati lepa rẹ
Arc aisedeede
Iṣatunṣe aibikita
Pupọ spatter
O tayọ alurinmorin ilana iṣẹ
Irin ti o dapọ ni awọn ohun-ini okeerẹ ti austenitic
ati irin alagbara, irin, ati ki o ni o tayọ pitting ati wahala ipata resistance
Ripple itanran
O dara fun alurinmorin ti biphase
irin alagbara, irin ti o ni 22% Cr ninu ile-iṣẹ petrochemical
Awọn microstructure weld jẹ austenitic - ferrite biphase be, ti o ni nipa 40% ferrite.
Rọrun slagging
Ọja Paramita
KỌMPUTA kemikali
ALOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | Miiran | |
GB/T OFIN | 0.04 | 0.5-2.0 | 1.00 | 21.0-24.0 | 7.5-10.0 | 2.5-4.0 | 0.04 | 0.03 | Ku: 0.75 / N: 0.08-0.20 | |
Aws ofin | 0.04 | 0.5-2.0 | 1.00 | 21.0-24.0 | 7.5-10.0 | 2.5-4.0 | 0.04 | 0.03 | Ku: 0.75 / N: 0.08-0.20 | |
APEERE IYE | 0.02 | 1 | 0.55 | 22.69 | 8.85 | 3.5 | 0.02 | 0.003 | Kù:0.02/N:0.11 |
Ohun-ini ẹrọ:
ONÍNÌYÀN | AGBARA YIELD(MPa) | AGBARA Ifaagun (MPa) | IMAPACT IYE J/℃ | ÌGBÀGBÀ(%) | ||||
GB/T OFIN | - | 690 | - | 15 | ||||
Aws ofin | - | 690 | - | 20 | ||||
APEERE IYE | - | 815 | 46/-20 | 26 |
Niyanju welding PARAMETER:
DIAMETERS PIPICATIONS(mm) | 1.2 | 1.6 | ||||||
Folti | 22-36 | 26-38 | ||||||
Amp | 120-260 | 200-300 | ||||||
Gigun itẹsiwaju gbigbe (mm) | 15-20 | 18-25 | ||||||
Ṣiṣan gaasi (l/min) | 15-25 | 15-25 |
Factory support
Ọja naa dara fun a
jakejado ibiti o ti ohun elo
WELDING TECHNOLOGY
Awọn ilẹkun mẹta 2 # ko ṣiṣẹ
CJ50 jack-soke lu
Awọn ohun elo alurinmorin fun awọn ọkọ ayọkẹlẹ iṣinipopada
KỌMPUTA kemikali
ALOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | Miiran | |
GB/T OFIN | 0.04 | 0.5-2.0 | 1.00 | 21.0-24.0 | 7.5-10.0 | 2.5-4.0 | 0.04 | 0.03 | Ku: 0.75 / N: 0.08-0.20 | |
Aws ofin | 0.04 | 0.5-2.0 | 1.00 | 21.0-24.0 | 7.5-10.0 | 2.5-4.0 | 0.04 | 0.03 | Ku: 0.75 / N: 0.08-0.20 | |
APEERE IYE | 0.02 | 1 | 0.55 | 22.69 | 8.85 | 3.5 | 0.02 | 0.003 | Kù:0.02/N:0.11 |
Ohun-ini ẹrọ:
ONÍNÌYÀN | AGBARA YIELD(MPa) | AGBARA Ifaagun (MPa) | IMAPACT IYE J/℃ | ÌGBÀGBÀ(%) | ||||
GB/T OFIN | - | 690 | - | 15 | ||||
Aws ofin | - | 690 | - | 20 | ||||
APEERE IYE | - | 815 | 46/-20 | 26 |
Niyanju welding PARAMETER:
DIAMETERS PIPICATIONS(mm) | 1.2 | 1.6 | ||||||
Folti | 22-36 | 26-38 | ||||||
Amp | 120-260 | 200-300 | ||||||
Gigun itẹsiwaju gbigbe (mm) | 15-20 | 18-25 | ||||||
Ṣiṣan gaasi (l/min) | 15-25 | 15-25 |