Awọn irin-kekere alloy Afọwọṣe elekiturodu E8018-C4 Mod data iṣelọpọ weld
KỌMPUTA kemikali
ALOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S |
GB/T OFIN | 0.10 | 1.25 | 0.80 | - | 1.10-2.00 | - | 0.03 | 0.03 |
Aws ofin | 0.10 | 1.25 | 0.80 | - | 1.10-2.00 | - | 0.03 | 0.03 |
APEERE IYE | 0.08 | 1.05 | 0.4 | 0.03 | 1.45 | 0.06 | 0.012 | 0.006 |
Ohun-ini ẹrọ:
ONÍNÌYÀN | AGBARA YIELD(MPa) | AGBARA Ifaagun (MPa) | IMAPACT IYE J/℃ | ÌGBÀGBÀ(%) | Itọju igbona °Cxh | |||||
GB/T OFIN | 460 | 550 | 27/-50 | 17 | 620*1 | |||||
Aws ofin | 460 | 550 | 27/-50 | 19 | 620*1 | |||||
APEERE IYE | 485 | 595 | 110/-50 | 25 | 620*1 | |||||
APEERE IYE | 490 | 602 | 108/-50 | 25 | AW |
Niyanju welding PARAMETER:
DIAMETERS PIPICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0 * 400 | 5.0 * 400 | ||||
ELECTRICITY (Amp) | H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||
O/W | 60-100 | 80-120 | 120-160 | - |
Irin lulú kekere hydrogen iru ọwọ elekiturodu.
Nitori awọn afikun ti irin lulú, awọn yo ṣiṣe jẹ ti o ga, awọn ikolu ti irin yo ni -50 ℃.
Idurosinsin aaki, kere asesejade, ti o dara lara, rorun slag yiyọ, X-Ray išẹ jẹ o tayọ.
-
400,000 toonu irin ti ngbe
-
Haiyang iparun agbara ọgbin
Sino-Russian Eastern Front
KỌMPUTA kemikali
ALOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S |
GB/T OFIN | 0.10 | 1.25 | 0.80 | - | 1.10-2.00 | - | 0.03 | 0.03 |
Aws ofin | 0.10 | 1.25 | 0.80 | - | 1.10-2.00 | - | 0.03 | 0.03 |
APEERE IYE | 0.08 | 1.05 | 0.4 | 0.03 | 1.45 | 0.06 | 0.012 | 0.006 |
Ohun-ini ẹrọ:
ONÍNÌYÀN | AGBARA YIELD(MPa) | AGBARA Ifaagun (MPa) | IMAPACT IYE J/℃ | ÌGBÀGBÀ(%) | Itọju igbona °Cxh | |||||
GB/T OFIN | 460 | 550 | 27/-50 | 17 | 620*1 | |||||
Aws ofin | 460 | 550 | 27/-50 | 19 | 620*1 | |||||
APEERE IYE | 485 | 595 | 110/-50 | 25 | 620*1 | |||||
APEERE IYE | 490 | 602 | 108/-50 | 25 | AW |
Niyanju welding PARAMETER:
DIAMETERS PIPICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0 * 400 | 5.0 * 400 | ||||
ELECTRICITY (Amp) | H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||
O/W | 60-100 | 80-120 | 120-160 | - |