AWS E9015-B3 iru ọwọ elekiturodu fun ooru sooro irin ni o dara fun ga otutu ati ki o ga titẹ opo gigun ti epo, sintetiki kemikali ẹrọ, Epo epo, ati be be lo, ṣiṣẹ ni isalẹ 550 ℃, gẹgẹ bi awọn 2.5Cr1Mo tube awo, A335-P22 tube, A387Gr. .22 awo.Tun le ṣee lo fun alurinmorin Cr2.5Mo kilasi (2.5CrMo, ati be be lo) pearlite ooru sooro, irin.Awọn alurinmorin isẹ ti jẹ DC yiyipada asopọ, ati ki o kikun ipo alurinmorin le wa ni ošišẹ ti, bi gun bi awọn preheating iṣẹ ṣaaju ki o to alurinmorin.A gba imọ-ẹrọ iṣelọpọ to ti ni ilọsiwaju, iṣakoso muna ni ipese ti awọn ohun elo aise, sisẹ ati iṣelọpọ, ayewo ọja, iṣẹ lẹhin-tita ti gbogbo alaye, lati pese awọn alabara pẹlu elekiturodu ti o dara julọ ati awọn iṣẹ okun waya.
Awọn ẹya ara ẹrọ
AWS E9015-B3 iru ọwọ alurinmorin elekiturodu fun ooru sooro irin ni a kekere soda hydrogen iru ọwọ alurinmorin elekiturodu, eyi ti o si tun ni o ni o tayọ irako resistance ni 550 ℃.Ati arc jẹ idurosinsin, kere si splashing, lara daradara, de-slagging jẹ rorun, X-Ray išẹ jẹ o tayọ;Labẹ awọn ipo itọju ooru pataki, o tun le rii daju iṣẹ ipa ipa iwọn otutu iduroṣinṣin.O tun le ṣee lo fun alurinmorin pearlite ooru sooro irin pẹlu titẹ ohun elo ṣiṣẹ otutu ni isalẹ 550 ℃, gẹgẹ bi awọn 12Cr2MolR ati awọn ohun elo miiran.Ṣaaju ki o to alurinmorin, o jẹ pataki lati san ifojusi si preheating awọn iwọn otutu laarin awọn ikanni si 160 ~ 190 ℃ ṣaaju ki o to alurinmorin.Lẹhin ti alurinmorin ti pari, ilana itọju ooru ti 690 ± 15 ℃ * 1h ni a ṣe ni ibamu si awọn ibeere boṣewa ti awọn ohun elo alurinmorin.Nigbati alurinmorin yi ni irú ti irin gbọdọ wa ni preheated, o lọra itutu lẹhin alurinmorin ati awọn miiran igbese, ṣugbọn awọn preheating otutu ni ko awọn ti o ga ti o dara, gbọdọ muna muse awọn ibeere ilana alurinmorin.
Ile-iṣẹ & Ile-iṣẹ
Ọja tiwqn ati darí-ini ifihan
KỌMPUTA kemikali
ALOY(wt%) | C | Mn | Si | Cr | Mo | P | S |
GB/T OFIN | 0.05-0.12 | 0.90 | 1.00 | 2.00-2.50 | 0.90-1.20 | 0.03 | 0.030 |
Aws ofin | 0.05-0.12 | 0.90 | 1.00 | 2.00-2.50 | 0.90-1.20 | 0.03 | 0.030 |
APEERE IYE | 0.075 | 0.76 | 0.36 | 2.26 | 1.08 | 0.011 | 0.007 |
Ohun-ini ẹrọ:
ONÍNÌYÀN | AGBARA YIELD(MPa) | AGBARA Ifaagun (MPa) | ÌTẸ̀RẸ̀YÌN ℃xh | IMAPACT IYE J/℃ | ÌGBÀGBÀ(%) | |||||||||
GB/T OFIN | 530 | 620 | 690*1 | - | 15 | |||||||||
Aws ofin | 530 | 620 | 690*1 | - | 17 | |||||||||
APEERE IYE | 576 | 692 | 690*1 | 150 / Iseda otutu, 138/0 | 19.5 |
Niyanju welding PARAMETER:
DIAMETERS PIPICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0 * 400 | 5.0 * 400 | ||||||
ELECTRICITY (Amp) | H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||||
O/W | 60-100 | 80-120 | 120-160 | - |
Awọn alaye Iṣakojọpọ:
ÌSÍPÍṢẸ́ | AGBO | PCS/1KG | ÌWÚN/1KG | |||
2.6mm | 300mm | 48PCS | 2KG | |||
3.2mm | 350mm | 27 PCS | 5KG | |||
4.0mm | 350mm | 16 PCS | 5KG | |||
5.0mm | 350mm | 12 PCS | 5KG |
AKIYESI:
H/W: alurinmorin ipo petele
O/W: alurinmorin ipo lori-ori
Awọn ọran Aṣoju
Iwe-ẹri
Ọja tiwqn ati darí-ini ifihan
KỌMPUTA kemikali
ALOY(wt%) | C | Mn | Si | Cr | Mo | P | S |
GB/T OFIN | 0.05-0.12 | 0.90 | 1.00 | 2.00-2.50 | 0.90-1.20 | 0.03 | 0.030 |
Aws ofin | 0.05-0.12 | 0.90 | 1.00 | 2.00-2.50 | 0.90-1.20 | 0.03 | 0.030 |
APEERE IYE | 0.075 | 0.76 | 0.36 | 2.26 | 1.08 | 0.011 | 0.007 |
Ohun-ini ẹrọ:
ONÍNÌYÀN | AGBARA YIELD(MPa) | AGBARA Ifaagun (MPa) | ÌTẸ̀RẸ̀YÌN ℃xh | IMAPACT IYE J/℃ | ÌGBÀGBÀ(%) | |||||||||
GB/T OFIN | 530 | 620 | 690*1 | - | 15 | |||||||||
Aws ofin | 530 | 620 | 690*1 | - | 17 | |||||||||
APEERE IYE | 576 | 692 | 690*1 | 150 / Iseda otutu, 138/0 | 19.5 |
Niyanju welding PARAMETER:
DIAMETERS PIPICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0 * 400 | 5.0 * 400 | ||||||
ELECTRICITY (Amp) | H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||||
O/W | 60-100 | 80-120 | 120-160 | - |
Awọn alaye Iṣakojọpọ:
ÌSÍPÍṢẸ́ | AGBO | PCS/1KG | ÌWÚN/1KG | |||
2.6mm | 300mm | 48PCS | 2KG | |||
3.2mm | 350mm | 27 PCS | 5KG | |||
4.0mm | 350mm | 16 PCS | 5KG | |||
5.0mm | 350mm | 12 PCS | 5KG |