Low-alloy steels Afowoyi elekiturodu E8018-C3 Soldering asopọ
KỌMPUTA kemikali
ALOY(wt%) | C | Mn | Si | Ni | Cr | Mo | V | P | S |
GB/T OFIN | 0.12 | 0.40-1.25 | 0.80 | 0.8-1.10 | 0.15 | 0.35 | 0.05 | 0.03 | 0.03 |
Aws ofin | 0.12 | 0.40-1.25 | 0.80 | 0.8-1.10 | 0.15 | 0.35 | 0.05 | 0.03 | 0.03 |
APEERE IYE | 0.07 | 1.02 | 0.4 | 1.02 | 0.05 | 0.05 | 0.003 | 0.012 | 0.007 |
Ohun-ini ẹrọ:
ONÍNÌYÀN | AGBARA YIELD(MPa) | AGBARA Ifaagun (MPa) | IMAPACT IYE J/℃ | ÌGBÀGBÀ(%) | Itọju igbona °Cxh | |||||
GB/T OFIN | 470-550 | 550 | 27/-40 | 20 | AW | |||||
Aws ofin | 470-550 | 550 | 27/-40 | 24 | AW | |||||
APEERE IYE | 495 | 585 | 135/-40 | 26 | AW |
Niyanju welding PARAMETER:
DIAMETERS PIPICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0 * 400 | 5.0 * 400 | ||||
ELECTRICITY (Amp) | H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||
O/W | 60-100 | 80-120 | 120-160 | - |
Irin lulú kekere hydrogen potasiomu iru ọwọ elekiturodu, nitori awọn afikun ti irin lulú, ga yo ṣiṣe.
Ipa lile ti irin didà ni -40 ℃ otutu iṣẹ jẹ dara julọ.
Idurosinsin aaki, kere asesejade, ti o dara lara, rorun slag yiyọ, X-Ray išẹ jẹ o tayọ.
-
Arctic LNG-2 ise agbese
-
Canada LNG Project
-
Shaanxi Pucheng -50 ℃ propane ojò ojò ise agbese
KỌMPUTA kemikali
ALOY(wt%) | C | Mn | Si | Ni | Cr | Mo | V | P | S |
GB/T OFIN | 0.12 | 0.40-1.25 | 0.80 | 0.8-1.10 | 0.15 | 0.35 | 0.05 | 0.03 | 0.03 |
Aws ofin | 0.12 | 0.40-1.25 | 0.80 | 0.8-1.10 | 0.15 | 0.35 | 0.05 | 0.03 | 0.03 |
APEERE IYE | 0.07 | 1.02 | 0.4 | 1.02 | 0.05 | 0.05 | 0.003 | 0.012 | 0.007 |
Ohun-ini ẹrọ:
ONÍNÌYÀN | AGBARA YIELD(MPa) | AGBARA Ifaagun (MPa) | IMAPACT IYE J/℃ | ÌGBÀGBÀ(%) | Itọju igbona °Cxh | |||||
GB/T OFIN | 470-550 | 550 | 27/-40 | 20 | AW | |||||
Aws ofin | 470-550 | 550 | 27/-40 | 24 | AW | |||||
APEERE IYE | 495 | 585 | 135/-40 | 26 | AW |
Niyanju welding PARAMETER:
DIAMETERS PIPICATIONS(mm) | 2.6*350 | 3.2*350 | 4.0 * 400 | 5.0 * 400 | ||||
ELECTRICITY (Amp) | H/W | 80-110 | 100-130 | 130-180 | 170-210 | |||
O/W | 60-100 | 80-120 | 120-160 | - |